Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
5455000 | Materials Characterization | 2016 | 42 Pages |
Abstract
Nanocrystalline Fe83.3Si3B10P3Cu0.7 alloys have a heterogeneous microstructure consisting of α-Fe nanocrystals with an average size of few tenths of nanometers and an amorphous residual phase. Nanocrystalline alloy annealed at 698 K has a saturated magnetic flux density of 1.81 T and coercivity of 11.8 A mâ 1. Its hetero-amorphous microstructure undergoes active dissolution in H2SO4, and α-Fe grains are preferentially dissolved in the form of micro-coupling cells between anodic α-Fe grains and cathodic amorphous residue and Cu clusters. Because the P enrichment in the residual phases inhibits the anodic dissolution of Fe and the α-Fe grains act as sacrificial anodes, the amorphous residual phases do not readily dissolve. The final residual phase is amorphous and has a nanoporous structure with a pore size similar to that of the precipitated α-Fe grains after annealing. The active dissolution behavior is determined by the microstructure of nanocrystalline Fe83.3Si3B10P3Cu0.7 alloys.
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Science (General)
Authors
Zhenhua Dan, Fengxiang Qin, Yan Zhang, Akihiro Makino, Hui Chang, Nobuyoshi Hara,