Abstract
The mechanical properties of zirconium hydrides were studied using nano-indentation technique between 25 and 400 °C. Temperature dependency of reduced elastic modulus and hardness of δ- and ε-zirconium hydrides were obtained by conducting nanoindentation experiments on bulk hydride samples with independently heating capability of indenter and heating stage. The reduced elastic modulus of δ-zirconium hydride (H/Zr ratio = 1.61) decreased from â¼113 GPa at room temperature to â¼109 GPa at 400 °C, while its hardness decreased significantly from 4.1 GPa to 2.41 GPa in the same temperature range. For ε-zirconium hydrides (H/Zr ratio = 1.79), the reduced elastic modulus decreased from 61 GPa at room temperature to 54 GPa at 300 °C, while its hardness from 3.06 GPa to 2.19 GPa.
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Metals and Alloys
Authors
M. Nedim Cinbiz, Mehdi Balooch, Xunxiang Hu, Aida Amroussia, Kurt Terrani,