Article ID Journal Published Year Pages File Type
5460798 Journal of Alloys and Compounds 2017 33 Pages PDF
Abstract
In this work, γ-butyrolactone (GBL) and glutaronitrile (GLN) are used as electrolyte additives for LiNi0.5Mn1.5O4 cathode of lithium ion battery. At 1 C rate, the capacity of LiNi0.5Mn1.5O4 is significantly improved by using 2% GBL as additive, its average capacity reaches 113 mA h g−1. In base electrolyte, the capacity is only 99.5 mA h g−1. However, utilizing 10% GLN just keeps the capacity around 110 mA h g−1 in first 50 cycles, and its final capacity is 32.3 mA h g−1. A series of tests indicate that GBL preferentially oxidized on LiNi0.5Mn1.5O4 forming a stable protective film, which prevents the subsequent oxidation decomposition of the electrolyte from taking place, on the contrary, although GLN has a wider electrochemical window, it can simply enable the cyclic stability at low current rate. When current is increased, the incompatibility of GLN with low voltage Li anode is enlarged.
Related Topics
Physical Sciences and Engineering Materials Science Metals and Alloys
Authors
, , , , ,