Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
5464562 | Surface and Coatings Technology | 2017 | 37 Pages |
Abstract
Ni-Ti-O nanoporous film with pore diameters of 60-75 nm are produced anodically on NiTi in ethylene glycol containing 5-10 vol% H2O and 0.15-0.3 M NaCl at 10-20 V. The film fabricated in the NaCl-containing electrolyte are much thinner than those prepared in the HCl-containing electrolyte under similar experimental conditions, implying proper amount of H+ in the electrolyte accelerates formation of the nanopores. Moreover, the experimental conditions to grow Ni-Ti-O nanoporous film on NiTi are not proper for pure Ti and Ni. The film of 1.9 μm in thickness exhibits good cytocompatibility thus is suitable for biomedical applications.
Related Topics
Physical Sciences and Engineering
Materials Science
Nanotechnology
Authors
Ruiqiang Hang, Yanlian Liu, Ang Gao, Mingxiang Zong, Long Bai, Xiangyu Zhang, Xiaobo Huang, Bin Tang, Paul K. Chu,