Ni-W/diamond composite coatings were prepared by electrodeposition from a Ni-W plating bath with diamond particles suspended into the bath. The effect of the plating parameters on microstructure and mechanical properties was investigated. The deposits reported a maximum hardness of 1207 ± 32 Hv. The film hardness is depended on the concentration of diamond particles in the plating bath and also on the size of the co-deposited diamond particles. The sample with diamond concentration of 10 g/L in the bath and co-deposited at current density of 0.15 A/cm2 reported the optimized wear resistance and diamond content in the deposit. In this paper the effect of the incorporation of diamond particles into the Ni-W matrix has been discussed in terms of the aforesaid operating conditions and particle size.
Related Topics
Physical Sciences and Engineering
Materials Science
Nanotechnology
Authors
Malay Kumar Das, Rongxia Li, Jiaqian Qin, Xinyu Zhang, Kumkumlata Das, Adisak Thueploy, Sarintorn Limpanart, Yuttanat Boonyongmaneerat, Mingzhen Ma, Riping Liu,