Abstract
The defect density calculation indicated that the defect density of HIPIMS/UBM coatings increased (from 0.48 to 3.18%) with the coating thickness. A coating produced in a relatively clean chamber had a lower defect density. Potentiodynamic polarisation experiments showed that the fluctuation in corrosion currents in HIPIMS/UBM coatings reduced with the coating thickness. This indicated that though visible on the surface, most of these defects did not penetrate thorough the whole thickness of the coating.