Post irradiated microstructural characterisation of pure Ti and Ti-6Al-4V has been done as a function of dose using different model based techniques of X-ray diffraction line profile analysis. There is a systematic change of domain size for both the materials with dose but the microstrain within the domain remains almost unaltered. The domain size appears to be lower for pure Ti at all doses as compared to Ti-6Al-4V alloy. XRD peaks became highly asymmetric particularly at a dose of 5Â ÃÂ 1021Â p/m2 for Ti-6Al-4V samples which is not observed for pure Ti at the same dose. This may be attributed to the segregation of alloying elements as a result of irradiation. Microhardness values increases with dose for pure Ti and then saturates at higher doses whereas microhardness values are found to decrease at higher doses for Ti-6Al-4V.
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Surfaces, Coatings and Films
Authors
A. Dutta Gupta, P. Mukherjee, N. Gayathri, P. Bhattacharyya, M. Bhattacharya, Apu Sarkar, S. Sen, M.K. Mitra,