Abstract
In the present work, the combination of mechanical alloying (MA) and spark plasma sintering (SPS) has been utilized to improve the hardness and strength of the Fe-20Mn-11Al-1.8C-5Cr quinary alloy displaying good corrosion resistance. The mechanically alloyed powders consisted of a primary body-center cubic (BCC) phase and a small amount of face-center cubic (FCC) phase, however, the sintered alloy was composed of γ matrix, k-carbide ((Fe, Mn)3AlCx) and Cr7C3 carbide. In addition, nanoscale twins presented in some γ grains after SPS. Vickers hardness of the sintered Fe-20Mn-11Al-1.8C-5Cr quinary alloy with ultra-fine grains (UFGs) is 705 HV, which is markedly higher than that of the as-cast Fe-20Mn-11Al-1.8C-5Cr counterparts. The compressive yield strength of the sintered samples at room temperature (RT) and at 873 K are 2339 MPa and 980 MPa, respectively, which are both significantly higher than those of their as-cast counterparts, suggesting that the ultra-fine grained Fe-20Mn-11Al-1.8C-5Cr alloy can be potentially used in corrosion-wear conditions at elevated temperatures.
Related Topics
Physical Sciences and Engineering
Materials Science
Surfaces, Coatings and Films
Authors
Jian Liu, Weiping Chen, Zhenfei Jiang, Lusheng Liu, Zhiqiang Fu,