Gold leaching from EW-PBC, using 0.4Â M Thiourea solutions at pH 1.5, during three hours. Pretreatment conditions: HCl: copper leaching for six hours with solution 0.5Â M HCl with air sparging. Citrate: copper leach for six hours with 0.5Â M citrate solution at pH 4.5 and addition of peroxide. M: Material without any preliminary treatment.88