Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
576957 | Journal of Hazardous Materials | 2014 | 8 Pages |
Abstract
Mixtures consisting of harbor sediment and slag waste from steel industry containing toxic components are fired to produce non-hazardous construction materials. The fired pellets become lighter as firing temperature increases. At a sintering temperature of â¦1050 °C, the fired pellets are in a form of brick-like product, while at 1100 °C, they become lightweight aggregates. Calcium silicate, kyanite, and cristobalite are newly formed in the pellets after firing, demonstrating that calcium oxide acts as a flux component and chemically reacted with Si- and/or Al-containing components to promote sintering. Dioxin/furan content present in the pure slag is 0.003 ng I-TEQ gâ1 and, for the fired pellet consisting of slag and sediment, the content appears to be destructed and diminishes to 0.0003 ng I-TEQ gâ1 after 950 °C-firing; while it is 0.002 ng I-TEQ gâ1 after firing at 1100 °C, suggesting that dioxins/furans in the 950 °C-fired pellets have a greater chance to escape to atmosphere due to a slower sintering reaction and/or that construction of dioxins/furans from molten chloride salts co-exists with their destruction. Multiple toxicity characteristic leaching procedure extracts Cu, Cr, Zn, Se, Cd, Pb, Ba, As, and Hg from all fired products at negligible levels.
Related Topics
Physical Sciences and Engineering
Chemical Engineering
Chemical Health and Safety
Authors
Yu-Ling Wei, Chang-Yuan Lin, Shao-Hsiang Cheng, H. Paul Wang,