578501 | Journal of Hazardous Materials | 2012 | 9 Pages |
Abstract
⺠The citrate precursor synthesized in leaching process is Pb(C6H6O7)·H2O. ⺠Orthorhombic lead oxide, Pb and amorphous C are the major calcination products of the Pb(C6H6O7)·H2O in nitrogen gas. ⺠Nanostructured leady oxide powders are obtained at 370 °C for 20 min calcination in air.