Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
585344 | Journal of Hazardous Materials | 2006 | 9 Pages |
Abstract
The results of TCLP showed that among the metals of Cr, Cd, Cu and Pb, only the concentrations of Pb in raw fly ash exceeded the regulation. At sintering temperatures of 700, 800 and 900 °C, the concentration of Pb decreased in sintering products, however, the concentration of Pb still exceeded the limitation at 700 and 800 °C. Additionally, the water-washing was used to pre-treat the fly ash before sintering process. The washing treatment effectively reduced the leaching concentrations of Pb to agree the regulations. Therefore, water-washing followed by a sintering treatment is an available process for detoxifying the fly ash of MSWI.
Related Topics
Physical Sciences and Engineering
Chemical Engineering
Chemical Health and Safety
Authors
Ming-Yen Wey, Kuang-Yu Liu, Tsung-Hsun Tsai, Jing-Tong Chou,