Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
6053153 | Journal of Dentistry | 2013 | 6 Pages |
Abstract
The failure mode and fracture origin of the GI restoratives tested using Hertzian indentation is representative of the clinical situation in vivo. The reliability of the load to failure data sets produced were improved compared with routinely employed mechanical testing approaches suggesting the possibility of inclusion as an ISO testing protocol.