Abstract
												⺠The lowest surface roughness value achieved for POM was 0.44 μm (45% decrease) and for PUR was 0.46 μm (42% decrease). ⺠The lowest coefficient of friction value achieved was 0.22 (32.9% decrease) for POM and 0.24 (28.8% decrease) for PUR. ⺠The lowest specific wear rate value achieved was 0.31Ã10â6 mm3/N m (38.6% decrease) for POM and 0.41Ã10â6 mm3/N m (37.9% decrease) for PUR.