Wear variations of Incoloy MA956 slid against Incoloy 800HT between room temperature and 750 °C, and sliding speeds of 0.314, 0.654 and 0.905 m s−1 were investigated using a ‘reciprocating block-on-cylinder’ (low debris retention) configuration.Three forms of wear depending largely on sliding temperature were observed: ‘severe wear’ with high transfer between room temperature and 270 °C, ‘severe wear’ with low transfer between 390 and 570 °C and ‘glaze formation’ (retarded by increased sliding speed) at 630 °C and above. The differences in wear behaviour are discussed, with wear behaviour mapped and wear surfaces at 750 °C (0.314 and 0.905 m s−1) cross-sectioned and profiled.