Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
617668 | Wear | 2013 | 9 Pages |
Abstract
The ultrathin DLC coatings with thickness of 2Â nm and 5Â nm were deposited onto Si(100) substrate by the filtered cathodic arc technique. The nanowear tests were performed on DLC coatings and Si(100) substrate by diamond tip and SiO2 microspheric tips. The results indicated that the coatings could support an indentation with a peak contact pressure of 7Â GPa. During scratch tests, the critical load corresponding to the generation of grooves on silicon substrate could be raised by 75%/125% after the deposition of DLC coating of 2Â nm/5Â nm in thickness. When the nanowear tests were conducted by a diamond tip, DLC coatings could effectively resist the mechanical wear and prevent the formation of hillock on silicon substrate. Moreover, since two DLC coatings present a close coverage on silicon substrate, they can largely resist the tribochemical wear of silicon substrate by SiO2 tip in humid air. Under a contact pressure of 1.3Â GPa, the wear depth on 2Â nm/5Â nm DLC coating was only 0.42Â nm/0.28Â nm, which was less than 5% of that on silicon substrate. Finally, either in humid air or in vacuum, 2Â nm DLC coating presented the excellent durability to protect the silicon substrate from wear damage. Therefore, although thicker DLC coating to some extent reveals better wear resistance, 2Â nm DLC coating is enough to protect its substrate against nanowear.
Keywords
Related Topics
Physical Sciences and Engineering
Chemical Engineering
Colloid and Surface Chemistry
Authors
L. Chen, M.C. Yang, C.F. Song, B.J. Yu, L.M. Qian,