Abstract
â¶ Fluoride ions hinder instantaneous repassivation of damaged areas of fretted zone. â¶ Adhesive galling is observed both in presence and in absence of fluoride ions. â¶ Wear volume is higher at 190Â ppm but lower at 570 and 1140Â ppm of fluoride ions. â¶ Change in contact configuration reduced the wear rate at 1140Â ppm of fluoride ions.