Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
620294 | Wear | 2006 | 19 Pages |
Abstract
The mechanisms that allowed the formation of this scale were determined. SEM observations in conjunction with EDS analysis, both inside and outside the contact area on both antagonists, led to the development of a phenomenological model explaining the creation and the movement of oxide debris in the contact.
Related Topics
Physical Sciences and Engineering
Chemical Engineering
Colloid and Surface Chemistry
Authors
C. Vergne, C. Boher, R. Gras, C. Levaillant,