Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
6501463 | Applied Catalysis B: Environmental | 2014 | 10 Pages |
Abstract
- Temperature rise from 350 to 700 °C causes gold-enrichment in the surface region of Au/Pd particles.
- Au/Pd-TiO2 calcined at 350 and 400 °C have higher activity than those calcined from 450 to 700 °C.
- For all Au/Pd-TiO2 samples, O
- â radical are mainly responsible for phenol degradation under UV.
- Visible light irradiation led to the formation of carbon radical at the Au/Pd-TiO2 surface.
Keywords
Related Topics
Physical Sciences and Engineering
Chemical Engineering
Catalysis
Authors
Anna Cybula, Jacqueline B. Priebe, Marga-Martina Pohl, Janusz W. Sobczak, Matthias Schneider, Anna ZieliÅska-Jurek, Angelika Brückner, Adriana Zaleska,