Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
6505487 | Catalysis Today | 2013 | 6 Pages |
Abstract
- Reactivity on Ni(1Â 1Â 1) was studied as a function of temperature.
- Substantial H2 formation is obtained at 1400Â K and 1600Â K.
- H2 molecules are the most frequently formed species at 1600Â K.
- Carbon diffusion into lower subsurface layers starts at a temperature of 1200Â K.
Related Topics
Physical Sciences and Engineering
Chemical Engineering
Catalysis
Authors
W. Somers, A. Bogaerts, A.C.T. van Duin, S. Huygh, K.M. Bal, E.C. Neyts,