Abstract
A three-dimensional carbon fiber cloth (CFC) is placed between the separator and the sulfur cathode to accommodate and capture the soluble polysulfide intermediates. The cells with this interlayer show an initial discharge capacity of 6.89 mAh cmâ2, which remains substantial after 100 cycles at 1C (6.69 mAh cmâ2).