Article ID Journal Published Year Pages File Type
6607291 Electrochimica Acta 2016 30 Pages PDF
Abstract
High quality MnO2/MnCo2O4 composites have been successfully synthesized by a one-step solution combustion process at 300 °C for 2 h in air. The effects of the amount of glycine and molar ratios of Mn/Co on phase composition, morphology and electrochemical properties of products were investigated. The prepared samples were characterized by X-ray diffraction, field-emission scanning electron microscopy, X-ray photoelectron spectroscopy, transmission electron microscopy and Brunauer-Emmett-Teller methods. Based on the optimum fuel/oxidizer molar ratios, the products transformed from spinel MnCo2O4 granular aggregates to a mixture of MnO2/MnCo2O4 composites with increase the molar ratios of Mn/Co. The electrochemistry performance of prepared different specimens were evaluated and compared through cyclic voltammetry and charge-discharge anylysis in 2.0 M KOH electrolytic solution. Electrochemical measurements showed that the MnO2/MnCo2O4 exhibited a optimal electrochemistry performance with the Mn:Co:glycine molar ratio of 3:4:31.5/9. The maximum specific capacitance of 497 F/g is achieved at a current density of 0.5 A/g (or 312 F/g at 10 A/g). The high electrochemical performance would be attributed to the numerous nanopores, large specific surface and synergistic effects of the MnO2 and spinel MnCo2O4.
Related Topics
Physical Sciences and Engineering Chemical Engineering Chemical Engineering (General)
Authors
, , , , , , , , ,