Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
6643485 | Fuel | 2012 | 8 Pages |
Abstract
⺠H2/CO can be varied from 0.9 to 4.2 by increasing calcite loading and S/B at 100% calcite loading. ⺠Change in calcite loading provides flexibility to meet required H2/CO in target applications. ⺠Total tar concentration decreased exponentially from 5.0 to 0.7 g/Nm3 with the calcite loading. ⺠Tar reduction from 0% to 50% calcite loading was found to be higher than that from 50% to 100% loading.
Related Topics
Physical Sciences and Engineering
Chemical Engineering
Chemical Engineering (General)
Authors
Woei L. Saw, Shusheng Pang,