Article ID Journal Published Year Pages File Type
6644305 Fuel 2012 8 Pages PDF
Abstract
► Polymeric materials exposed to E20 showed mass increases below 10%. ► Ethanol absorption by some polymers is due to the high affinity of the amide group with the hydroxyl group. ► Some polymers displayed a greater hardness decrease in samples immersed in gasoline than samples immersed in the E20. ► There were changes in the crystallinity of the PA66 after being exposed to both fuels.
Related Topics
Physical Sciences and Engineering Chemical Engineering Chemical Engineering (General)
Authors
, , ,