The steam exploded pellets saw the lowest drop in mechanical durability (5%) but saw the largest decrease in shear modulus, whilst the white wood pellets disintegrated in situ after 4 days. In contrast storage at 10% RH did not cause any observable degradation, with mechanical behaviour of steam exploded and torrefied pellets showing an improvement. This paper presents both testing methodology as well as clear indication of the behaviour of three woody biomass pellets on exposure to high relative humidity.