Abstract
In this paper, the refinement of low-grade ilmenite concentrate was studied. It was found that by transforming in NaOH/NaNO3 molten salt, and then leaching in water and in dilute hydrochloric acid, the low-grade ilmenite concentrate containing 3.09â¯wt% Mg, 1.03â¯wt% Ca, 3.38â¯wt% Si and 1.54â¯wt% Al can be refined well, meanwhile the contents of Ti and Fe are not affected. The lattice of ilmenite concentrate can be completely destroyed in the molten salt with NaOH/NaNO3 weight ratio 7:3 at 400â¯Â°Cfor 6â¯h. The removal rates of Mg, Al, Ca and Si are 86.62%, 90.55%, 92.62%, 92.90% respectively by leaching the transformed concentrate in water with L/S ratio 2:1â¯mL/g at 60â¯Â°C for 0.5â¯h, and leaching the water leached residue in dilute HCl solution with L/S ratio 4:1â¯mL/g under pHâ¯1.2 at 40â¯Â°C for 2â¯h. The contents of Mg, Al, Ca and Si are 0.41â¯wt%, 0.13â¯wt%, 0.08â¯wt% and 0.21â¯wt% respectively in the refined concentrate, which is suitable for arc reduction smelting to produce high-quality titanium slag.
Keywords
Related Topics
Physical Sciences and Engineering
Chemical Engineering
Chemical Engineering (General)
Authors
Xuewen Wang, Xuehui Liu, Yiqian Ma, Mingyu Wang, Yi Wang, Xingming Wang,