Article ID Journal Published Year Pages File Type
6673754 Minerals Engineering 2013 8 Pages PDF
Abstract
► We integrate NaHS sulfidization with lime neutralization for selective recovery of Cu and Zn over Fe from AMD. ► Adding more than 20 mg/L NaHS at pH 2.8 without pH adjustment could selectively precipitate Cu over Fe and Zn. ► Fe could be precipitated over Zn afterward by lime neutralization at pH 5 whereas the addition of oxidizing agent was needed. ► Adding 10-15 mg/L NaHS could selectively precipitate Cu over Zn at pH 5 after Fe was fully precipitated by lime previously.
Related Topics
Physical Sciences and Engineering Chemical Engineering Chemical Engineering (General)