Article ID Journal Published Year Pages File Type
672292 Particuology 2008 6 Pages PDF
Abstract

For the first time dry roller vibration milling at room temperature was used to prepare active carbon (AC) nano-particles and to modify MnO2 powder as electrode materials. In 30 min AC was milled to a mean particle size of 30–50 nm with increased crystallinity and higher specific surface area, predominantly mesoporous and with improved pore diameter distribution. Then, AC nano-particles were incorporated with MnO2 or bismuth-doped MnO2 nano-particles synthesized by sol–gel methods to prepare nano-composite electrode materials for studying their electrochemical performance. The AC nano-particles combined with 10 wt.% bismuth-doped MnO2 nano-particles were found to possess excellent electrochemical property with specific capacitance up to 308 F/g and without obvious attenuation with increasing current. Our method seems to open a new way to improve AC based electrode materials used for clean energy such as super capacitors.

Related Topics
Physical Sciences and Engineering Chemical Engineering Fluid Flow and Transfer Processes
Authors
, , ,