Abstract
⺠102 Samples of carbonate rocks were tested during 100 cycles of freeze-thaw. ⺠Decay evolution was characterized at micro/meso-scale and petrophysically. ⺠Ultrasonic attenuation is the most useful parameter for studying damage evolution. ⺠Strength, porosity and weight decrease are not useful for damage quantification. ⺠Standard procedures are revealed as not effective for rock durability diagnostics.