Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
6743234 | Fusion Engineering and Design | 2018 | 6 Pages |
Abstract
In this paper, tungsten films were deposited on tungsten substrates by magnetron sputtering and some films were annealed at 1273â¯K for 1â¯h. Subsequently, the morphology and microstructure of as-deposited and pre-annealed films were measured by scanning electron microscopy and X-ray diffraction. In addition, both films were exposed to helium ions with energy of 60â¯keV and fluence of 1.0â¯Ãâ¯1022â¯mâ2 at room temperature. After helium irradiation, the blisters formed on surface of films induced by helium irradiation were observed by scanning electron microscopy. Here we report the differences in blistering on surface between as-deposited and pre-annealed films. In addition, in spite of similar microstructure of both films including grain size and preferred orientation, the different compressive stresses within both films lead to the different behaviors of blistering.
Related Topics
Physical Sciences and Engineering
Energy
Energy Engineering and Power Technology
Authors
Jiangang Yu, Wenjia Han, Zhe Chen, Kaigui Zhu,