Article ID Journal Published Year Pages File Type
6744362 Fusion Engineering and Design 2017 6 Pages PDF
Abstract
In this paper, W-0.5 wt.% Ta-0.01 wt.% C (W-05Ta-001C) alloys were fabricated via a combination of high energy ball milling and subsequent spark plasma sintering. The W-05Ta-001C alloys showed high strength of 565 MPa at 400 °C with a total elongation of 54%. The improved ductility resulted from nanosized TaC precipitation. The microstructure analysis of W-05Ta-001C alloys indicate that the nanosized TaC precipitation uniformly distributed in the grain interior encouraging trapping dislocations. TaC could reduce free oxygen concentration and thus enhance grain boundaries strength by reacting with impurities of oxygen to form compounds of Ta-Cx-Oy at grain boundaries. The thermal stability of W-05Ta-001C alloys was investigated by analyzing the evolution of hardness based on isochronal annealing tests. The results showed that hardness only slightly decreased with increasing annealing temperature up to 1500 °C, and the recrystallization temperature was about 1600 °C. This good thermal stability is attributed to nanosized TaC dispersion strengthened structures.
Related Topics
Physical Sciences and Engineering Energy Energy Engineering and Power Technology
Authors
, , , , , , , , ,