Abstract
Replacing of Ni as activator element by Pd for W/W or W/steel joints was achieved and joining with Cu-filler was successfully performed. Manufactured joints were characterized applying metallurgical testing and SEM/EDX analyses demonstrating the applicability of Pd activator. First shear tests showed that the joints exhibit mechanical stability sufficient for technical application.