Electrical connectors need to display low and stable electrical contact resistance (ECR). However, subjected to vibrations (engines, heat, etc.), fretting wear damages promotes the formation of insulating oxide debris and a sharp ECR increase decaying the information transmission. Noble plated coatings like silver layers are usually applied to delay the ECR failure. However, to predict such ECR endurance, it appears essential to determine the fretting wear rate. In the present study, a homogeneous crossed-cylinders Ag/Ag interface was investigated under gross slip conditions imposing various loading parameters (±2 µm<δg<±16 µm, 1 N4 mΩ) can be formalized, using a power law function of the mean friction energy density dissipated during a fretting cycle taking into account the contact area extension. Finally, a simple ECR endurance expression is derived as a function of the fretting loading parameters and the thickness of the silver plated layer. A very good correlation between experimental and predicted ECR endurances is achieved.
Related Topics
Physical Sciences and Engineering Chemical Engineering Colloid and Surface Chemistry
Authors
, , ,