Abstract
⺠Defects show a negative impact on the interfacial strength. ⺠V2N shows lower resistance to interfacial spalling than VN. ⺠VN shows the lowest resistance to interfacial fatigue. ⺠V2N shows the lowest critical normal load for interfacial spalling. ⺠Defects show a strong influence on material pick-up of the counter material.