Article ID Journal Published Year Pages File Type
7167635 Engineering Failure Analysis 2018 11 Pages PDF
Abstract
Failure happened to a 316LN stainless steel elbow pipe of the nuclear power plant (NPP) located at south China. Detailed analysis has been made to figure out the mode and root cause. Non-destructive tests, chemical composition analysis, mechanical property tests, scanning electronic microscopy, energy spectrum and micro-structure analyses, and cold-work elongation analysis have been conducted. Results reveal lots of cold-work slip bands exist in the microstructure. Deformation coefficient is about 32% in the crack regime. The hardness is 390 HV0.1, and cracks present brittle characteristics and propagate along the grain boundary. Furthermore, the fracture possesses crystal characteristics. Thus, indicate failure of elbow pipe occurs due to inter-granular stress corrosion cracking (IGSCC) that penetrates the whole pipe wall, and the root cause of elbow pipe failure is the high-cold-work condition.
Related Topics
Physical Sciences and Engineering Engineering Industrial and Manufacturing Engineering
Authors
, , , , , , , , ,