Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7172294 | International Journal of Fatigue | 2014 | 8 Pages |
Abstract
Based on the fracture surfaces observations, the developing fatigue-crack always initiated at the advancing side, namely on the boundary between the nugget and the thermo-mechanically affected zone into the interior of the specimen.
Keywords
Related Topics
Physical Sciences and Engineering
Engineering
Mechanical Engineering
Authors
Catarina Vidal, VirgÃnia Infante, Pedro Vilaça,