Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7175170 | International Journal of Pressure Vessels and Piping | 2015 | 9 Pages |
Abstract
In the present investigation, systematic studies on microstructure and mechanical properties of P92 steel subjected to various normalizing (1313-1353Â K) and tempering (1013-1053Â K) temperatures were carried out. The effect of heat treatment on microstructural parameters revealed an increase in grain size, lath width and decrease in the area fraction of the precipitates with an increase in normalizing temperature. The precipitate size has not changed significantly with increase in the normalizing temperature; rather it increased with increase in tempering temperature. Activation energy calculations confirmed the two fold mechanisms that dominate the tempering behavior. As a consequence, yield stress (YS) and ultimate tensile strength (UTS) were found to change with normalizing and tempering temperatures. P92 steel normalized at 1353Â K and tempered at 1013Â K was found to have the best combination of strength and ductility.
Related Topics
Physical Sciences and Engineering
Engineering
Mechanical Engineering
Authors
Dipika R. Barbadikar, G.S. Deshmukh, L. Maddi, K. Laha, P. Parameswaran, A.R. Ballal, D.R. Peshwe, R.K. Paretkar, M. Nandagopal, M.D. Mathew,