7208097 | Journal of the Mechanical Behavior of Biomedical Materials | 2016 | 53 Pages |
Abstract
- HA-Si-MWCNTs coating was fabricated on NiTi implant using electrophoretic deposition.
- HA-Si-MWCNTs coating has highest normal load before failure during scratch test.
- HA-Si-MWCNTs coating shows elastic modulus of 45.8Â GPa between NiTi and bone tissue.
- Presence of both Si and MWCNTs in HA coating induce more adherence of viable hMSCs.