Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7223215 | Optik - International Journal for Light and Electron Optics | 2018 | 9 Pages |
Abstract
ZnGa2O4:Yb3+,Er3+ and ZnAl2O4:Yb3+,Er3+ up-conversion powder phosphors with different Yb/Er ratio are synthesized by solid-state method and subsequent thermal treatment at 1300â¯â, which can generate strong up-conversion emissions in visible spectral range under 980â¯nm excitation. For the as-prepared ZnGa2O4:Yb3+,Er3+ phosphors, the green and red emissions around 524â¯nm (corresponding to 2H11/2â¯ââ¯4I15/2 transition of Er3+), 549â¯nm (corresponding to 4S3/2â¯ââ¯4I15/2 transition of Er3+) and 659â¯nm (corresponding to 4F9/2â¯ââ¯4I15/2 transition of Er3+) indicate the optimal Yb/Er ratio for the sample is 7/1, while the ZnAl2O4:Yb3+,Er3+ phosphors with the same green and red emissions is Yb/Erâ¯=â¯3/1. Besides the up-conversion luminescence, the morphology and crystal structure are also investigated. All ZnGa2O4:Yb3+,Er3+ powders contain regular long rods with diameter of about 600-900â¯nm, while agglomerates composed of nonregular particles with size about 200-400â¯nm are shown in all ZnAl2O4:Yb3+,Er3+ powders. Additionally, all samples are spinel structure with a high degree of crystallinity. Consequently, the particles of moderate size, stable crystal structure and enough high intensity of green and red emissions in all ZnGa2O4:Yb3+,Er3+ and ZnAl2O4:Yb3+,Er3+ powder phosphors endow them potential applications in infrared detection, display devices and so on.
Keywords
Related Topics
Physical Sciences and Engineering
Engineering
Engineering (General)
Authors
Yuan Cheng, Kangning Sun, Pinghui Ge,