Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7746323 | Solid State Ionics | 2014 | 4 Pages |
Abstract
Electro-catalytic nanoparticles can be produced in oxide anodes for solid oxide fuel cell (SOFC) by an ex-solution method, i.e., by incorporating metals into a perovskite oxide phase in air followed by the reduction of the perovskite oxide. In this study, we used a Ni ex-solution method with a La and Ni co-doped SrTiO3 (La0.2Sr0.8Ti1 â xNixO3 â δ, x = 0-0.2) anode for SOFC. The parameters and mechanisms of the Ni ex-solution were investigated by varying the ex-solution temperature (800-1300 °C) and time (3-24 h). The degrees of Ni ex-solution and Ti reduction were dependent on time and temperature. Ni ex-solution reaction was relatively faster than Ti reduction which required a higher temperature or a longer time. XRD analysis was used to observe the changes in the lattice parameter of La0.2Sr0.8Ti1 â xNixO3 â δ after the ex-solution process. The electrochemical performance of an electrolyte (Sc-stabilized zirconia)-supported cell with the La0.2Sr0.8Ti1 â xNixO3 â δ anode with x = 0.1 showed that the total cell resistance is high, due mostly to the anode resistance. The maximum power density at 800 °C is also relatively low, ~ 150 mW/cm2, due to the thick (~ 300 μm) electrolyte and the low level of anodic performance.
Related Topics
Physical Sciences and Engineering
Chemistry
Electrochemistry
Authors
Byung Hyun Park, Gyeong Man Choi,