Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7825333 | Polymer Testing | 2018 | 30 Pages |
Abstract
Elastomers are usually mechanically reinforced with high loadings of carbon black (CB) to achieve the properties demanded; high amounts of mineral flame retardants are used to fulfill fire safety requirements. In this study, multilayer graphene (MLG), a nanoparticle made of only 10 graphene sheets, is applied in low loadings, 3 parts per hundred rubber (phr) to reduce the total amount of filler or boost performance in hydrogenated acrylonitrile-butadiene rubber (HNBR). In the HNBR/MLG nanocomposites, 3 phr MLG replaced 15 phr CB, 3 phr aluminum trihydroxide (ATH), or 15 phr CBÂ +Â 3 phr ATH. The nanocomposites were prepared via master batch by ultrasonically assisted solution mixing and subsequent conventional two-roll milling. A comprehensive study is presented, illustrating the impact of MLG on curing and mechanical properties; e.g. replacing 2.5 phr ATH with 3 phr MLG increased the Young's modulus by over 60% and hardness by 10%, while improving flame retardancy, and reducing the total heat evolved by 10%. MLG is a multifunctional filler, as demonstrated by various enhancements in terms of the mechanical and flame retardancy properties of the rubber composites.
Keywords
Related Topics
Physical Sciences and Engineering
Chemistry
Organic Chemistry
Authors
Benjamin Zirnstein, Weronika Tabaka, Daniele Frasca, Dietmar Schulze, Bernhard Schartel,