Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7839800 | Journal of Luminescence | 2018 | 7 Pages |
Abstract
BaLu1.94Al4SiO12:0.06Ce3+ (BLASO:0.06Ce3+) green-emitting phosphor could be easily obtained by a conventional solid-state reaction method at 1400â¯Â°C. BLASO:0.06Ce3+ possesses the garnet structure (Ia3Ì
d space group) with the lattice parameter aâ=â11.9222(0) Ã
. The emission peak of BLASO:0.06Ce3+ is located at 513ânm and its photoluminescent quantum yield is determined to be 92.4% at 25â°C when excited at 450ânm. BLASO:0.06Ce3+ presents excellent thermal properties, with the photoluminescence intensity at 200â°C only decreased to 91.5% of its room temperature value. A phosphor-converted white LED device fabricated by using BLASO:0.06Ce3+ as the green phosphor exhibits good optical performance with Raâ=â88.5, CCTâ=â3562 K and CIE1931 chromaticity coordinates as (xâ=â0.4041, yâ=â0.3951). The results indicate that BLASO:0.06Ce3+ phosphor has strong potential applications in developing high color rendering, thermally stable, warm-white LEDs.
Keywords
Related Topics
Physical Sciences and Engineering
Chemistry
Physical and Theoretical Chemistry
Authors
Yaochun Qiang, Zhifang Pan, Xinyu Ye, Mingzhang Liang, Jianfei Xu, Jianhui Huang, Weixiong You, Huali Yuan,