Article ID Journal Published Year Pages File Type
7858934 Dental Materials 2018 9 Pages PDF
Abstract
In general, the addition of QAS increased composite's degradation compared with the CG. In the tested QAS, the addition of DMADDM at 5% concentration resulted in a less degradable material.
Related Topics
Physical Sciences and Engineering Materials Science Biomaterials