Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7875718 | Acta Materialia | 2018 | 31 Pages |
Abstract
(Left) Plot of steady-state strain rate vs. applied stress for compression creep tests at 700â¯Â°C showing that adding 1.5 or 2â¯wt%Ti to a Fe-Ni-Al-Cr ferritic steel drastically increases creep resistance. When further adding 0.5â¯wt% Hf, the creep resistance drops. (Right) Dark-field TEM micrograph of Ti- and Hf-modified steel aged at 700â¯Â°C showing B2 precipitates (green) containing L21 sub-precipitates (red).316
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
Sung-Il Baik, Michael J.S. Rawlings, David C. Dunand,