Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
787692 | International Journal of Pressure Vessels and Piping | 2006 | 6 Pages |
Abstract
In TAGSI's view re-characterisation needs to be considered separately for contained plastic collapse and ductile or brittle fracture of the remaining ligament. For plastic collapse and ductile tearing of the remaining ligament the R6 rules for re-characterisation appear generally satisfactory. For brittle failure of the ligament in many cases the R6 recommendations will be found satisfactory but for cases of large difference between static and dynamic toughness it is recommended that scoping calculations should be carried out for the defect geometry, loading and material properties of concern.
Keywords
Related Topics
Physical Sciences and Engineering
Engineering
Mechanical Engineering
Authors
F.M. Burdekin, A.H. Sherry,