Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7880005 | Acta Materialia | 2015 | 8 Pages |
Abstract
Fully amorphous rods with diameters up to 2Â mm diameter were obtained upon 0.5Â at.% Cu addition to the Fe36Co36B19.2Si4.8Nb4 bulk metallic glass. The Cu-added glass shows a very good thermal stability but, in comparison with the Cu-free base alloy, the entire crystallization behavior is drastically changed. Upon heating, the glassy (Fe36Co36B19.2Si4.8Nb4)99.5Cu0.5 samples show two glass transitions-like events, separated by an interval of more than 100Â K, in between which a bcc-(Fe,Co) solid solution is formed. The soft magnetic properties are preserved upon Cu-addition and the samples show a saturation magnetization of 1.1Â T combined with less than 2Â A/m coercivity. The relaxation behavior prior to crystallization, as well as the crystallization behavior, were studied by time-resolved X-ray diffraction using synchrotron radiation. It was found that both glassy alloys behave similar at temperatures below the glass transition. Irreversible structural transformations take place when approaching the glass transition and in the supercooled liquid region.
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
Mihai Stoica, Parthiban Ramasamy, Ivan Kaban, Sergio Scudino, Mircea Nicoara, Gavin B.M. Vaughan, Jonathan Wright, Ravi Kumar, Jürgen Eckert,