Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7887275 | Ceramics International | 2018 | 6 Pages |
Abstract
We fabricated xBaTiO3 (BT)/(1-x)[BaTiO3-Bi(Mg1/2Ti1/2)O3-BiFeO3] (BT-BMT-BF)â¯+â¯0.1â¯wt%MnCO3 composites by spark plasma sintering and investigated the effect of BT content x, BT powder size, and BT-BMT-BF composition on piezoelectric properties. For xBT/(1-x)(0.3BT-0.1BMT-0.6BF) +â¯0.1â¯wt%MnCO3 (xâ¯=â¯0-0.75) composites with a 0.5-µm BT powder, the dielectric constant was increased with x, and the relative density was decreased at xâ¯=â¯0.67 and 0.75, creating optimum BT content of xâ¯=â¯0.50 with a piezoelectric constant d33 of 107â¯pC/N. When a larger 1.5-µm BT powder was utilized for the composite with xâ¯=â¯0.50, the d33 value increased to 150â¯pC/N due to the grain size effect of the BT grains. To compensate for a compositional change from the optimum 0.3BT-0.1BMT-0.6BF due to partial diffusion between the BT and 0.3BT-0.1BMT-0.6BF grains, a 0.5BT/0.5(0.275BT-0.1BMT-0.625BF)â¯+â¯0.1â¯wt%MnCO3 composite with the 1.5-µm BT powder was fabricated. We obtained an increased d33 value of 166â¯pC/N. These results provided a useful composite design to enhance the piezoelectric properties.
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
Ichiro Fujii, Shin Ariizumi, Shintaro Ueno, Chikako Moriyoshi, Yoshihiro Kuroiwa, Satoshi Wada,