Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7888091 | Ceramics International | 2018 | 19 Pages |
Abstract
C/C-ZrC and C/SiC-ZrC composites were fabricated by a joint process of slurry impregnation and chemical vapor infiltration, in which ZrC matrix was obtained by slurry impregnation process, while C or SiC matrix was introduced by chemical vapor infiltration process. The as fabricated C/C-ZrC and C/SiC-ZrC composites have densities of 1.67 g cmâ3 and 1.91 g cmâ3 respectively. Tensile strength is 89.4±8.4 MPa and 182.2±14.0 MPa respectively for the as prepared C/C-ZrC and C/SiC-ZrC. Ablation behavior of the C/C-ZrC and C/SiC-ZrC composites under air plasma was studied and compared in detail. Due to different oxidation resistance and heat transfer capacity of the matrix, these two ZrC based composites showed various ablation behavior. The linear erosion rate is 48 µm sâ1 and 39 µm sâ1 respectively for C/C-ZrC and C/SiC-ZrC composites.
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
Haijun Zhou, Dewei Ni, Ping He, Jinshan Yang, Jianbao Hu, Shaoming Dong,