Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7889832 | Composites Part A: Applied Science and Manufacturing | 2018 | 31 Pages |
Abstract
The experimental test results show high potential for detecting defects in FMLs. Delamination, which occurs between the glass fibre/matrix interface, can be electrically detected using the capacitance measurement. The fracture surface of the pre-treated metal sheet demonstrates that the adhesive bond between the cubical hook-like surface structure of the aluminium and the matrix remains intact.
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
Björn Bosbach, Christoph Ohle, Bodo Fiedler,