Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7895337 | Corrosion Science | 2015 | 22 Pages |
Abstract
To increase the oxidation resistance of carbon/carbon (C/C) composites at high temperature, it was modified by ZrB2-SiC ceramics with precursor infiltration and pyrolysis process, then SiC coating was prepared on the modified composites by pack cementation. The results show that the SiC coating prepared with Si/C weight ratio of 6:0.5 has better oxidation resistance, It can effectively protect C/C composites for 100 h at 1773 K with the weight gain per unit area of 7.75 g cmâ2. The good oxidation resistance of the coated composites is attributed to the formation of dense SiO2 glass during the oxidation test.
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
Yu-Lei Zhang, Tian Fei, Wen-Ying Zeng, Bo-Xing Yang, He-Jun Li, Ke-Zhi Li,